Automotive heat reveals which 3D printed materials actually survive. PLA softens near 60°C and fails in a hot car, while ABS handles interior heat and ASA handles exterior sun and UV.
In this episode you'll learn:
- ABS has a glass transition around 105°C and parts work long-term at roughly 80 to 90°C, while PLA starts softening at 50 to 60°C.
- ABS density ranges from 0.9 to 1.53 g/cm3 with a median of 1.07 g/cm3, and thermal conductivity sits around 0.1 W/(m K).
- ASA replaces ABS's butadiene with an acrylate elastomer, which resists UV photo-oxidation that yellows and embrittles ABS outdoors.
- ASA tensile strength is about 33 MPa and Izod impact strength around 321 J/m, comparable to ABS (30 to 40 MPa, 200 to 400 J/m).
- ASA Heat Deflection Temperature reaches up to 93°C per Prusament data, in the same band as ABS (80 to 98°C).
Read the full guides on our site: ASA: Outdoor Alternative to ABS Without Compromise · ABS Production Guide: When and Why to Choose It Over PLA
Watch on YouTube: 3D Printing Made Easy playlist
We 3D-print custom props and game pieces for Z-AGENCY and TerraHunt.
This show is our AI bonus channel: episodes are automatically generated audio editions of the articles we publish at printara3d.com, so you can follow our topics on the go.
Fler avsnitt
Visa alla avsnitt av 3D Printing Made Easy3D Printing Made Easy med Printara 3D finns tillgänglig på flera plattformar. Informationen på denna sida kommer från offentliga podd-flöden.